厂家及牌号 | 试验条件 | 测试方法 | 线形热膨胀系数-流动(-30到30°C) |
POM共聚 沙伯基础 LNP™ LUBRICOMP™ KAL22M compound (润滑,耐磨损性良好,注射成型填料:芳族聚酰胺纤维, 10% 填料按重量。) | ASTMD696 | 9.9E-5 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ LUBRICOMP™ KL003 compound | ASTMD696 | 1.1E-4 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ LUBRICOMP™ KFL36 compound | ASTMD696 | 9.5E-5 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ LUBRICOMP™ KFI12 compound (耐磨损性良好,润滑,注射成型填料:玻璃纤维增强材料, 10% 填料按重量。) | ASTMD696 | 8.3E-5 cm/cm/°C | |
此文献版权所有.请勿转载或其它用途.http://pbtsl.com/ | |||
POM共聚 沙伯基础 LNP™ LUBRICOMP™ KL003LH compound (耐磨损性良好,低萃取物,润滑,注射成型) | ASTMD696 | 1.3E-4 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ STAT-KON™ KS000MXL compound (金属探测,低萃取物填料:不锈钢纤维。) | ASTMD696 | 9.9E-5 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ THERMOCOMP™ KF005 compound (化学耦合,注射成型填料:玻璃纤维增强材料, 25% 填料按重量。) | ASTMD696 | 7.1E-5 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ THERMOCOMP™ KB006 compound (共聚物,注射成型填料:玻璃珠, 30% 填料按重量。) | ASTMD696 | 8.3E-5 cm/cm/°C | |
POM共聚 沙伯基础 LNP™ THERMOCOMP™ KZ002 compound (注射成型填料:带压花的玻璃纤维, 10% 填料按重量。) | ASTMD696 | 1.1E-4 cm/cm/°C | |
温馨提示 | |||
1.有关“线形热膨胀系数-流动(-30到30°C) POM共聚”类数据资讯最多展示10条.更多牌号应用数据请向客服索取。 2.有关“POM共聚塑料原料价格”类数据的实时性及更多塑料原料价格行情敬请关注我们的资讯动态. |