| 厂家及牌号 | 试验条件 | 测试方法 | 装有测量仪表的落镖冲击 |
| PPO(PPE)+PS 沙伯基础 NORYL™ SE100HX resin (无溴,阻燃性,无氯,注射成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 3.28 J |
| PPO(PPE)+PS 沙伯基础 NORYL™ SE100X resin | -30°C,EnergyatPeakLoad | ASTMD3763 | 16.3 J |
| PPO(PPE)+PS 沙伯基础 NORYL GTX™ GTX626 resin (高耐热性,耐化学性良好,挤出吹塑成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 36.6 J |
| PPO(PPE)+PS 沙伯基础 NORYL™ PPX640 resin (延高的拉伸率,高刚性注射成型填料:玻璃纤维增强材料, 40% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 14.1 J |
| 此文献-版权所有-请勿转载或其它用途.http://pbtsl.com/ | |||
| PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX630 resin | -30°C,TotalEnergy | ASTMD3763 | 20.4 J |
| PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX630F resin (高刚性,延高的拉伸率,注射成型填料:玻璃纤维增强材料, 30% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 20.4 J |
| PPO(PPE)+PS 沙伯基础 NORYL GTX™ GTX902 resin (耐化学性良好,可喷涂的,注射成型) | -40°C,EnergyatPeakLoad | ASTMD3763 | 19.7 J |
| PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX640F resin (延高的拉伸率,高刚性注射成型填料:玻璃纤维增强材料, 40% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 14.1 J |
| PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX830 resin | -30°C,TotalEnergy | ASTMD3763 | 10.0 J |
| PPO(PPE)+PS 沙伯基础 NORYL GTX™ GTX910 resin (耐化学性良好,尺寸稳定性良好,注射成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 39.5 J |
| 温馨提示 | |||