厂家及牌号 | 试验条件 | 测试方法 | 熔流率(熔体流动速率)(300°C/5.0kg) |
PPO(PPE)+PS 沙伯基础 NORYL™ HNA055 resin | ASTMD1238 | 6.2 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ NH7010HF resin | ASTMD1238 | 20 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ EFN4230 resin (高耐热性) | ASTMD1238 | 14 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ PKN4775F resin (,高ESCR(抗应力开裂),高耐热性,片材挤出成型) | ASTMD1238 | 15 g/10min | |
此文献版权所有,请勿转载或其它用途.http://pbtsl.com/ | |||
PPO(PPE)+PS 沙伯基础 NORYL™ CN5260 resin (阻燃性填料:填料, 50% 填料按重量。) | ASTMD1238 | 13 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ GFN3 resin | ASTMD1238 | 8.7 g/10min | |
PPO(PPE)+PS 美国PTS PTS PPE-LXS314-30 (抗撞击性高填料:玻璃纤维增强材料, 30% 填料按重量。) | ASTMD1238 | 15 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ CRX1005 resin (耐化学性良好) | ASTMD1238 | 14 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ GFN2F resin | ASTMD1238 | 9.0 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ GFN2 resin | ASTMD1238 | 9.0 g/10min | |
温馨提示 | |||
1.有关“熔流率(熔体流动速率)(300°C/5.0kg) PPO(PPE)+PS”类数据资讯最多展示10条.更多牌号应用数据请向客服索取。 2.有关“PPO(PPE)+PS塑胶原料”类数据的实时性及更多塑胶原料行情敬请关注我们的资讯动态. |
● ABS UnnotchedIzodImpactStrength3(23°C)
● EVA 拉伸模量-100%
● PC 弯曲应力(3.5%应变)
● ECTFE 摩擦系数(与自身-动态)
● PPO(PPE)+PS 悬壁梁缺口冲击强度(3.20mm)