厂家及牌号 | 试验条件 | 测试方法 | 熔流率(熔体流动速率)(280°C/5.0kg) |
PPO(PPE)+PS 沙伯基础 NORYL™ EXNL0357 resin (阻燃性,无卤,注射成型) | ASTMD1238 | 9.6 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL GTX™ GTX934 resin (可加工性良好,良好的耐热老化性能,注射成型) | ASTMD1238 | 13 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ LS6010 resin | ASTMD1238 | 5.7 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ NH5020 resin | ASTMD1238 | 9.8 g/10min | |
此文献版权所有,请勿转载-或其它用途.http://pbtsl.com/ | |||
PPO(PPE)+PS 沙伯基础 NORYL™ BN9003G resin (抗撞击性良好,优良外观,挤出吹塑成型) | ASTMD1238 | 10 g/10min | |
PPO(PPE)+PS 韩国LG化学 Lumiloy® GN1306F (通用,阻燃性,高耐热性,注射成型) | ASTMD1238 | 8.0 g/10min | |
PPO(PPE)+PS 韩国LG化学 Lumiloy® GP2300 (抗撞击性高,水解稳定,通用,注射成型填料:玻璃纤维增强材料, 30% 填料按重量。) | ASTMD1238 | 9.0 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ PVX0901 resin (通用,注射成型) | ASTMD1238 | 50 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL GTX™ GTX985 resin (可喷涂的,导电性,高耐热性,高刚性注射成型填料:矿物填料, 18% 填料按重量。) | ASTMD1238 | 16 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ N1150 resin | ASTMD1238 | 15 g/10min | |
温馨提示 | |||
1.有关“熔流率(熔体流动速率)(280°C/5.0kg) PPO(PPE)+PS”类数据资讯最多展示10条.更多牌号应用数据请向客服索取。 2.有关“PPO(PPE)+PS塑料颗粒”类数据的实时性及更多塑料颗粒行情敬请关注我们的资讯动态. |
● PBT VolumeResistivity(1.50mm)
● LDPE 肖氏硬度
● PBT/ASA 相对漏电起恒指数CTI
● PTFE 拉伸强度
● PC+ABS UnnotchedIzodImpactStrength3(23°C)