厂家及牌号 | 试验条件 | 测试方法 | UnnotchedIzodImpactStrength3(23°C) |
PEEK 沙伯基础 LNP™ LUBRICOMP™ LL004 compound | ISO180/1U | 91 kJ/m2 | |
PEEK 沙伯基础 LNP™ THERMOCOMP™ LC006 compound | ISO180/1U | 43 kJ/m2 | |
PEEK 沙伯基础 LNP™ THERMOCOMP™ LF008 compound | ISO180/1U | 54 kJ/m2 | |
PEEK 沙伯基础 LNP™ LUBRICOMP™ LCL33 compound | ISO180/1U | 35 kJ/m2 | |
此文献版权所有,请勿转载-或其它用途.http://pbtsl.com/ | |||
PEEK 沙伯基础 LNP™ THERMOCOMP™ LF006 compound | ISO180/1U | 57 kJ/m2 | |
PEEK 沙伯基础 LNP™ THERMOCOMP™ LC003E compound | ISO180/1U | 29 kJ/m2 | |
PEEK 沙伯基础 LNP™ THERMOCOMP™ LC008E compound | ISO180/1U | 40 kJ/m2 | |
PEEK 沙伯基础 LNP™ LUBRICOMP™ LCL33E compound | ISO180/1U | 35 kJ/m2 | |
PEEK 沙伯基础 LNP™ THERMOCOMP™ LF006E compound (良好的成型性能,注射成型填料:玻璃纤维增强材料, 30% 填料按重量。) | ISO180/1U | 59 kJ/m2 | |
PEEK 沙伯基础 LNP™ LUBRICOMP™ LL004C compound | ISO180/1U | 91 kJ/m2 | |
温馨提示 | |||
1.有关“UnnotchedIzodImpactStrength3(23°C) PEEK”类数据资讯最多展示10条.更多牌号应用数据请向客服索取。 2.有关“PEEK塑料颗粒”类数据的实时性及更多塑料颗粒行情敬请关注我们的资讯动态. |
● PMMA 泊松比
● LLDPE 断裂应力
● PC+PBT 抗张强度(屈服,23°C)
● PS 熔流率(熔体流动速率)(230°C/2.16kg)
● PC/ABS 热变形温度(0.45MPa,未退火)