厂家及牌号 | 试验条件 | 测试方法 | 熔流率(熔体流动速率)(260°C/5.0kg) |
PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX7110 resin | ASTMD1238 | 11 g/10min | |
PPO(PPE)+PS 沙伯基础 LNP™ LUBRICOMP™ Noryl_NWR5810 compound | ASTMD1238 | 5.5 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ RN0401 resin | ASTMD1238 | 30 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL™ PPX640 resin (延高的拉伸率,高刚性注射成型填料:玻璃纤维增强材料, 40% 填料按重量。) | ASTMD1238 | 1.3 g/10min | |
该文献版权所有.请勿.转载或其它用途.http://pbtsl.com/ | |||
PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX630 resin | ASTMD1238 | 2.6 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX630F resin (高刚性,延高的拉伸率,注射成型填料:玻璃纤维增强材料, 30% 填料按重量。) | ASTMD1238 | 2.6 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX7200 resin | ASTMD1238 | 16 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX640F resin (延高的拉伸率,高刚性注射成型填料:玻璃纤维增强材料, 40% 填料按重量。) | ASTMD1238 | 1.3 g/10min | |
PPO(PPE)+PS Generic Generic PPE+PS+PP | ASTMD1238 | 11到16 g/10min | |
PPO(PPE)+PS 沙伯基础 NORYL PPX™ PPX7115F resin (抗撞击性高,高耐热性,注射成型) | ASTMD1238 | 14 g/10min | |
温馨提示 | |||
1.有关“熔流率(熔体流动速率)(260°C/5.0kg) PPO(PPE)+PS”类数据资讯最多展示10条.更多牌号应用数据请向客服索取。 2.有关“PPO(PPE)+PS塑料原料价格”类数据的实时性及更多塑料原料价格行情敬请关注我们的资讯动态. |
● PS 无缺口悬臂梁冲击(23°C)
● PS 光泽度(60°)
● HIPS UL 阻燃等级
● PUR-MDI 维卡软化温度
● PA+PPO(PPE) 载荷下热变形温度(1.8MPa,未退火,3.18mm)